Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5304
I am experiencing issues with the chipwave of this machine. ... - Jun 06, 2007 by rm14
So you are saying that, for a CHIP wave (not the smooth, lam... - Jun 07, 2007 by Samir Nagheenanajar
Chip waves are supposed to be turbulant. You have 2 waves, ... - Jun 07, 2007 by Hussman
Man the only ripple i like to see is some fine cognac or he... - Jun 07, 2007 by Peter Gibbons
2 waves is correct. While running the glass test panel over ... - Jun 08, 2007 by rm14
Turbulant wave will get into the close quarter areas of your... - Jun 08, 2007 by Hussman
From my past experience, you can usually get away with OUT t... - Jun 08, 2007 by Dirk Nuendyke