Can it handle 0402 ? ... - Mar 20, 2007 by quanta
Yes, but you can expect a 20%+ pickup failure rate. Chuck... - Mar 20, 2007 by
You need to use the H nozzle and 4 small jaws (1005). Have... - Mar 21, 2007 by Darby
I did convert YM 84V for 0402, base on my expperience , this... - Mar 21, 2007 by