Hi all, I do know a little on PCB manufacturing. I would ... - Jul 29, 2006 by
The issue is not the gold, but the amount of gold. Gold con... - Jul 29, 2006 by davef
Davef is right about the amount, but why are using gold to s... - Jul 29, 2006 by
Thank you for your help. Using gold is not my decision, it i... - Jul 30, 2006 by Ali Uzel
OK so you're stuck with gold. Not all that bad unless you'r... - Jul 31, 2006 by
Ali Uzel