Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4134
I am curious if everyone else is seeing the same dramaticall... - May 02, 2006 by
You are exactly right, tip life is greatly reduced with the... - May 02, 2006 by RDR
I also heard that fluxes are more agressive in lead free all... - May 02, 2006 by Choppy
Sheldon, Try using SN100C wire solder. It seems to extend t... - May 03, 2006 by
Sheldon, Tip life is directly related to temperature, IR... - May 12, 2006 by
Just come back from Nepcon (electronics show on an obscure l... - May 12, 2006 by Rob
If you can change to SN100C do it. The nickel prevents the h... - May 12, 2006 by Steve
Hi Steve, Although your opinion is valid, calling somethi... - May 15, 2006 by Rob
Since when is Hakko putting more plating on their tips? I w... - May 15, 2006 by muse
Sheldon Stewart (Process Engineer)