Date: January 19, 2012 01:15 PM
Author: Steve
Subject: choices for SN100C for reflow

As a distributor we sell very little SN100C for SMT, we sell far more SAC305 for SMT. The higher temperatures are the reasons.


(http://www.smtnet.com/Forums/Index.cfm?CFApp=1&Message_ID=65764)



Login to SMTnet

Login or Register on SMTnet

Join SMTnet!


  • SMTnet
  • »
  • Login or Register on SMTnet

You must accept cookies in order to login to SMTnet.

Please turn cookies on, close this browser window and then return to SMTnet in order to allow SMTnet to verify that you have received a cookie.

Email Us with your questions or comments

  • SMTnet
  • »
  • Login or Register on SMTnet

  Post Reply
Author:
E-mail: Register Now   if you want users to be able to contact you.
Subject:
Message:

I want to use fixed-width font to display this message
Notify me by e-mail about all messages posted in this thread

automated test equipment for PCB test
Aquanox® A4638 - electronic assembly and advanced packaging cleaning agent
Now Online

351
Visitors

0
Members

Featured Companies
 

Electronic Testing, Semiconductor, SMT / PCB Auction