Subject: QFN soldering

Yes, but no guarantee of solderability. This just puts more paste on the pads. From my experience, unsoldered QFN parts are not due to lack of solder, but reflow.


(http://www.smtnet.com/Forums/Index.cfm?CFApp=1&Message_ID=66119)



Login to SMTnet

Login or Register on SMTnet

Join SMTnet!


  • SMTnet
  • »
  • Login or Register on SMTnet

You must accept cookies in order to login to SMTnet.

Please turn cookies on, close this browser window and then return to SMTnet in order to allow SMTnet to verify that you have received a cookie.

Email Us with your questions or comments

  • SMTnet
  • »
  • Login or Register on SMTnet

  Post Reply
Author:
E-mail: Register Now   if you want users to be able to contact you.
Subject:
Message:

I want to use fixed-width font to display this message
Notify me by e-mail about all messages posted in this thread

SMT Equipment Exchange Auction
SMT Chip Mounters
Now Online

326
Visitors

1
Members

Featured Companies