Hi, we have ERSA flow selective machine. We are using 420s-lf No-Clean flux (lead free process). It is water based. Before that we used for about 2 years in JS-EU-31 (KOKI) (alcohol based). It did excellent job (we moved to water based flux just because environmentally issues).