Hi,

That's good news, and we did outs with SN100C as well on Wed, however we are still working hard on getting a good profile.

We have some large BNC connectors, and they are hard to profile. We also have wave palettes, and these might be too thick, and causing variability, due to the temperature of them when they are loaded.

We are working on it now, and I am glad yours is working well!