What is the name of the dross eliminator you are referring to? Who is the manufacturer? I went to your website and didn't see anything about it? I just ordered some MS2 from P. Kay Metal as I've been hearing some very good things about it from longtime friends in the industry. One of my friends reduced his lead free solder purchases 80% and says he has absolutely no dross when using MS2. He did some cross sections before implementing and saw better hole fill as well. With the cost and difficulty's of Lead Free this is very appealing.