Converting your machine from lead to lead-free can be performed in a few steps: 1)Ensure the solder bath is up to temperature 2)De-dross the solder bath 3)Remove pumps/ flow ducts; etc. clean very well- set aside 4)Purge leaded solder 5)Remove as much solder/dross/other contaminants as possible 6)Fill solder pot with tin 7)Heat up, install pumps / flow ducts and cycle pumps to leach remaining lead) 8)Repeat steps 1~5 9)Fill with SN100C
if you have any specific questions, or require further information regarding SN100C, or your upcoming conversion, please feel free to contact me off-line.
Regards Jim